| MOQ: | 100pcs |
| Delivery Period: | Regional Depends |
| Payment Method: | T/T,Western Union |
| Supply Capacity: | 10000pcs per Month |
| Standard MR MDF | HMR MDF Pro |
|---|---|
| Passes 24h immersion (≤12% swell) | Validated under cyclic humidity testing (85% RH, 30°C x 7 days) |
| Wax added post-blending | Wax emulsified at fiber level for uniform distribution |
| Swells at edges after cutting | Stable edge integrity—even unsealed for 72h in humid air |
| Generic UF resin | Hybrid MUF+PF resin system with hydrolytic stability |
| Region | Challenge | Our Solution |
|---|---|---|
| Southeast Asia | Year-round >80% RH | High-density core + anti-fungal additive package |
| Middle East | AC condensation + dry heat cycling | Low EMC drift, minimal warpage |
| Northern Europe | Steam from cooking/bathing | Rapid moisture release without swelling |
| North America | Seasonal humidity swings | Stable across 30-80% RH range |
| MOQ: | 100pcs |
| Delivery Period: | Regional Depends |
| Payment Method: | T/T,Western Union |
| Supply Capacity: | 10000pcs per Month |
| Standard MR MDF | HMR MDF Pro |
|---|---|
| Passes 24h immersion (≤12% swell) | Validated under cyclic humidity testing (85% RH, 30°C x 7 days) |
| Wax added post-blending | Wax emulsified at fiber level for uniform distribution |
| Swells at edges after cutting | Stable edge integrity—even unsealed for 72h in humid air |
| Generic UF resin | Hybrid MUF+PF resin system with hydrolytic stability |
| Region | Challenge | Our Solution |
|---|---|---|
| Southeast Asia | Year-round >80% RH | High-density core + anti-fungal additive package |
| Middle East | AC condensation + dry heat cycling | Low EMC drift, minimal warpage |
| Northern Europe | Steam from cooking/bathing | Rapid moisture release without swelling |
| North America | Seasonal humidity swings | Stable across 30-80% RH range |